Carbon cast iron and Zinc coated steel were the most widely used portable water of supply and distribution Pipeline system. The leaching of red water in portable water could produce sericus environmental sanitary problems. Due to the red water was the most alternative to inner scale of metal pipeline. So this study was conducted the impact of red water on scale products, and was evaluated by the corrosive metal contaminants of 20 fears over. Surface tests, metal surface composition measurements of samples XRF, XRD, and SEM(EDS), analysis were used to investigate the corrosion characteristies of carbon cast iron and Zinc coated steel. As the contaminants of Fe increased the red water of carbon castiron pipe increased due to the scale products amount of $Fe_2O_3$ (Hemite).