  • 재습윤제의 적용이 상아질 접착에 미치는 효과
저자명
조영곤,박일윤,이영곤,Cho. Young-Gon,Park. Yil-Yoon,Lee. Young-Gon
간행물명
大韓齒科保存學會誌
권/호정보
2003년|28권 1호|pp.11-22 (12 pages)
발행정보
대한치과보존학회
파일정보
정기간행물|
PDF텍스트
주제분야
기타
이 논문은 한국과학기술정보연구원과 논문 연계를 통해 무료로 제공되는 원문입니다.
서지반출

기타언어초록

This study compared the dentin adhesion to composite resin according to air-dry, blot dry, application of rewetting agent on air-dry or blot dry dentin surface by microleakag test and SEM observation. For microleakage test, class V cavity preparations with dentinal margins were prepared on both buccal and lingual surfaces of 40 extracted human molars. For SEM observation, occlusal dentin of 20 extracted human molars were exposed. After etched the dentin, prepared teeth were randomly divided into four groups; D group: air dry for 10-15 sec., B group: blot dry with moist cotton pellet, D-R group: air dry and rewet with Aqua-Prep F for 20 sec., B-R group: blot dry and rewet with Aqua-Prep F for 20 sec. Treated cavities and surfaces were filled or constructed using One-Step adhesives and Aelitefil composite resins. Specimens were stored in distilled water for 24 hours. For microleakage test, the specimens were thermocycled and soaked into 2% methylene blue. The specimens were sectioned longitudinally and evaluated for microleakage under steromicroscope. The data were statistically analysed by Kuskal-Wallis Test, Mann-Whitney and Wilcoxon signed ranked tests. For SEM observation, the specimens were bisectioned mesiodiatally. After decalcified and deproteinized, specimens were observed under SEM. The results of this study were as follows; 1. The microleakges on dentinal margin were the highest in D group compared with B group, D-R group, and B-R group(p<0.05). But there was no significant difference between B group, D-R group and B-R group. 2. D group showed gap and a few resin tags between dentin and composite resin. 3 B group, D-R group, and B-R groups showed close adaptation between dentin and composite resin. It showed that resin rags in B group were numerous and long, in D-R group were few and short, in B-R group were numerous and short or long. 4. Adhesive layer showed in D-R group ($10{;}mu extrm{m}$) and B-R group ($3{;}mu extrm{m}$) In conclusion, use of rewetting agent to dry dentin was efficient to dentin adhesion, also it did not provide reverse effect on blot dry dentin.