도재라미네이트 접착용 레진시멘트의 색조 안정성에 관한 연구
[STEP1]서지반출 형식 선택
파일형식
@
서지도구
SNS
기타
[STEP2]서지반출 정보 선택
  • 제목
  • URL
돌아가기
확인
취소
  • 도재라미네이트 접착용 레진시멘트의 색조 안정성에 관한 연구
  • A STUDY ON THE COLOR STABILITY OF RESIN CEMENTS LUTED FOR PORCELAIN LAMINATE VENEER
저자명
김영운,박하옥,방몽숙,양홍서,박상원,Kim. Young-Woon,Park. Ha-Ok,Vang. Mong-Sook,Yang. Hong-So,Park. Sang-Won
간행물명
대한치과보철학회지
권/호정보
2007년|45권 2호|pp.191-202 (12 pages)
발행정보
대한치과보철학회
파일정보
정기간행물|
PDF텍스트
주제분야
기타
이 논문은 한국과학기술정보연구원과 논문 연계를 통해 무료로 제공되는 원문입니다.
서지반출

기타언어초록

Statement of problems: Long-term success of esthetic restorations, depends on various factors, especially on color stability of the restorations. The color stability is affected by resin cements beneath the porcelain laminate veneers. Purpose: The purpose of this study was to comprehend the color stability of resin cements by comparing with 4 different kinds of resin cements (Choice, Variolink II, Nexus 2, Rely-X). Material and methods: Porcelain laminate disk samples were luted with resin cements. After thermocycling of each 1000, 2000 and 3000 cycle, specimens were measured by spectrophotometers and the color differences were. Results: 1. After thermocycling of 1000, 2000 and 3000cycle, color difference, $({Delta}E^*)$ of all specimens were incresed, but were not statiscally significant differences. 2. In the Choice of A1 shade and the Nexus 2 of A3 shade, color difference$({Delta}E^*)$ after thermocycling of 3000cycle was $incre^*ased$ significantly than after thermocycling of 1000cycle. However, other groups did not show any statistically significant differences (P<0.05). 3. After thermocycling of 3000cycle, color difference$({Delta}E^*)$ between A1 shade and A3 shade of Nexus 2 showed statistically significant difference. However no statistically significant differences were observed in other groups (P<0.05). 4. The mean of color difference$({Delta}E^*)$ is 1.0-2.06 after 3000 thermocycling and the data were ranked in the ascending order of Variolink II, Nexus 2, Choice and Rely-X in A1 shade group and Choice, Rely-X, Variolink II and Nexus 2 in A3 shade group. Conclusion: Above results revealed that, after 3000 thermocycing, the color difference $({Delta}E^*)$ of experimental resin cements was within clinically acceptable ranges. Color stability of 4 different resin cements was comparatively excellent.