The authors have published several technical reports on the deterioration of conductor due to forest fire in series so far. This is because even we have been experiencing hundreds of forest fires every year, no systematic research on conductor which is very vulnerable to fire have been fulfilled. This paper describes the sag-tension behavior of conductor under loading current normally when only partial area of a long conductor is exposed to fire. Temperatures of Overhead Conductor were different with measurement position. When the partial area of conductor was heated up to $500^{circ}C$, 20 % of permanent tension loss was observed. This results in the increase of sag of 1.5 m when span is 300 m. The other results will be presented in the text.