초고강도 콘크리트의 수직, 수평부재 현장적용성을 위한 역학적 특성에 관한 연구
[STEP1]서지반출 형식 선택
파일형식
@
서지도구
SNS
기타
[STEP2]서지반출 정보 선택
  • 제목
  • URL
돌아가기
확인
취소
  • 초고강도 콘크리트의 수직, 수평부재 현장적용성을 위한 역학적 특성에 관한 연구
저자명
이근배,김성덕,백민수,정상진,Lee. Keun-Bae,Kim. Seong-Deok,Baek. Min-Su,Jung. Sang-Jin
간행물명
大韓建築學會論文集 : Journal of the architectural institute of Korea : Structure & construction / 構造系
권/호정보
2011년|27권 8호|pp.105-112 (8 pages)
발행정보
대한건축학회
파일정보
정기간행물|
PDF텍스트
주제분야
기타
이 논문은 한국과학기술정보연구원과 논문 연계를 통해 무료로 제공되는 원문입니다.
서지반출

기타언어초록

The vertical-horizontal separated placement method (V.H. separated placement method) is being widely used for high-rise buildings as well as for general buildings. The V.H. separated placement is advantageous in that the placement is easy, e.g., using vibrating compaction, because there is no interference of slab reinforcements in the case of concrete placement for columns, and that it allows forms to be easily removed and used for the next placement section. Despite the advantages of the V.H. separated placement, the V.H. concurrent placement is used in korea to reduce the construction period, which has the self compaction property and a high viscosity that prevents segregation. In this study, the basic data for concurrent placement of the high-strength concrete, including the transport properties, the strengths of members by height, and the hydration properties, were presented with concrete specimens with different strengths. The curing methods and core strengths for members in different locations met the targeted strengths, which were 60 MPa, 80 MPa and 100 MPa, at the given aging level. The core strength increased with aging. High increase in the strength was observed especially on the lower parts of the beams and columns. As for the strength of the core by height, the strength was higher on the middle and upper sections than on the lower sections, though the differences were not significant. With the increase in the targeted strength, the peak hydration temperature was reached in a shorter time, and the temperature difference between the center and surface of the specimen was about $15^{circ}C$ for each strength value.