콘크리트 포장용 고내구성 대체 다웰바의 실내공용성 평가
[STEP1]서지반출 형식 선택
파일형식
@
서지도구
SNS
기타
[STEP2]서지반출 정보 선택
  • 제목
  • URL
돌아가기
확인
취소
  • 콘크리트 포장용 고내구성 대체 다웰바의 실내공용성 평가
저자명
박성태,박준영,이재훈,김형배,Park. Seong Tae,Park. Jun Young,Lee. Jae Hoon,Kim. Hyung Bae
간행물명
한국도로학회논문집
권/호정보
2013년|15권 1호|pp.23-36 (14 pages)
발행정보
한국도로학회
파일정보
정기간행물|
PDF텍스트
주제분야
기타
이 논문은 한국과학기술정보연구원과 논문 연계를 통해 무료로 제공되는 원문입니다.
서지반출

기타언어초록

PURPOSES: The problem under this circumstance is that the erosion not only drops strength of the steel dowel bar but also comes with volume expansion of the steel dowel bar which can reduce load transferring efficiency of the steel dowel bar. To avoid this erosion problem, alternative dowers bars are developed. METHODS: In this study, the bearing stresses between the FRP tube dowel bar and concrete slab are calculated and compared with its allowable bearing stress to check its structural stability in the concrete pavement. These comparisons are conducted with several cross-sections of FRP tube dowel bars. Comprehensive laboratory tests including the shear load-deflection test on a full-scale specimen and the full-scale accelerated joint concrete pavement test are conducted and the results were compared with those from the steel dowel bar. RESULTS: In all cross-sections of FRP tube dowel bars, computed bearing stresses between the FRP tube dowel bar and concrete slab are less than their allowable stress levels. The pultrusion FRP-tube dowel bar show better performance on direct shear tests on full-scale specimen and static compression tests at full-scale concrete pavement joints than prepreg and filament-winding FRP-tube dowel bar. CONCLUSIONS: The FRP tube dowel bars as alternative dowel bar are invulnerable to erosion that may be caused by moisture from masonry joint or bottom of the pavement system. Also, the pultrusion FRP-tube dowel bar performed very well on the laboratory evaluation.