- CAD/CAM 전용 금속 합금과 주조용 합금의 세라믹 결합강도에 관한 연구
- ㆍ 저자명
- 정효경,곽동주,Jung. Hyo-Kyung,Kwak. Dong-Ju
- ㆍ 간행물명
- 대한치과기공학회지
- ㆍ 권/호정보
- 2013년|35권 2호|pp.89-95 (7 pages)
- ㆍ 발행정보
- 대한치과기공학회
- ㆍ 파일정보
- 정기간행물| PDF텍스트
- ㆍ 주제분야
- 기타
Purpose: The purpose of this study was to evaluate bond strength of Metal Disk alloy and casting alloy. Methods: Metal specimens were divided into 4 groups for each alloy. Three point flexural test were used to measure the bond strength of CAD/CAM metal alloy and casting alloy. Statistical analysis was done using the Statistical Package for Social Sciences version 19.0 for Windows. As for the analysis methods, the study used Kruskal-Wallis test. Results: The average bonding strengths of Group 1 to porcelain was $36.7{pm}9.90$ MPa, Group 2 to porcelain was $37.68{pm}4.51$ MPa, Group 3 to porcelain was $36.43{pm}6.57$ MPa, Group 4 to porcelain was $42.88{pm}6.81$ MPa, Each group was not significantly different. Conclusion: Bond strength of Casting alloy is equal to or higher than bond strength of CAD/CAM Metal Disk alloy. Alloy clinical bond strength is 25 MPa, So CAD/CAM Metal Disk alloy can be used as dental material.